sao tome and principe Plastic Pond Liner Geomembrane 0.5mm 0.75mm 1mm 1.5mm HDPE Geomembrane Liner
Category:
sao tome and principePond Liner
Product Description
Introduction
High Density Polyethylene (HDPE) is the high density version of PE plastic and is harder and denser than the LDPE, but is less ductile, and lighter than water. Climax HDPE Film / Sheet / Liner / Geomembrane has proved to be a boon especially for developing countries like India by playing an important role to prevent the air and groundwater pollution. The best thing is that it can be easily moulded and welded together and the use of UV Stabilizers improves its weather resistance. High Density Polyethylene Geomembrane lives up to the expectations which are demanded in today's world of environmental engineering. Climax HDPE's prime motive is to keep the Nature clean.
Video Showcase
Applications
1.landfill,sewage or control the waste residue seashores seepage.
2.Lake dam,tailings dams,sewage dam and reservoir,channel,storage of liquid pools(pit,ore)
3.The subway ,tunnel,anti-seepage lining of basement and tunnel.
4.To control the roadbed and other foundation saline seepage.
Working Drawing
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
Specifications
| Thicknesses mm | 0.75 | 1 | 1.25 | 1.5 | 2 | 2.5 | 3 |
| Densities g/cm³ | ≥ 0.940 | ||||||
| Roughness height | ≥0.25 | ||||||
| Tensile yield strength (longitudinal and transverse) N/mm | ≥11 | ≥15 | ≥18 | ≥22 | ≥29 | ≥37 | ≥44 |
| Tensile breaking strength (longitudinal and transverse) N/mm | ≥8 | ≥10 | ≥13 | ≥16 | ≥21 | ≥26 | ≥32 |
| Yield elongation (longitudinal and transverse) % | ≥12 | ||||||
| Elongation at break (longitudinal and transverse) % | ≥100 | ||||||
| Right angle tearing load (longitudinal and transverse) N | ≥93 | ≥125 | ≥160 | ≥190 | ≥250 | ≥315 | ≥375 |
| puncture strength N | ≥ 200 | ≥ 270 | ≥335 | ≥400 | ≥ 535 | ≥670 | ≥800 |
| Stress cracking under tensile load | ≥300 | ||||||
| Carbon black content % | 2.0-3.0 | ||||||
| Carbon Black Dispersibility | No more than 1 out of 10 data at level 3, not allowed at levels 4 and 5 | ||||||
| Atmospheric pressure oxidation induction time (OIT)min | Atmospheric pressure oxidation induction time ≥ 100 | ||||||
| High pressure oxidation induction time ≥ 400 | |||||||
| 85°C heat aging % | ≥55 | ||||||
| anti-ultraviolet | ≥ 50 | ||||||
Pack and Ship
Packaging: Standard packaging or customer's requirements
Lead time: Within 10-15 days after receiving the deposit payment
Producing Capacity: Two 40ft Containers per week
![]() |
![]() |
![]() |
![]() |