Papua New Guinea Textured HDPE Geomembrane

Geomembranes use plastic movies as anti-seepage substrates, commonly which encompass polyvinyl chloride (PVC) and polyethylene (PE), EVA (ethylene/vinyl acetate copolymer). In tunnel applications, ECB (ethylene vinyl acetate modified asphalt combo geomembrane) is moreover designed and used.

Category:

Papua New GuineaTextured HDPE Geomembrane

Product Description

Introduction

Geomembranes use plastic movies as anti-seepage substrates, commonly which encompass polyvinyl chloride (PVC) and polyethylene (PE), EVA (ethylene/vinyl acetate copolymer). In tunnel applications, ECB (ethylene vinyl acetate modified asphalt combo geomembrane) is moreover designed and used. They are immoderate molecular weight chemical flexible components with small special gravity, sturdy extensibility, immoderate adaptability to deformation, corrosion resistance, low temperature resistance, and excellent frost resistance.

Video Showcase

 

Applications

Applied to the projects of Landfill site, bank, dam, storage reservoir, channel, irrigation, highway, railway, tunnel, drinking tank, salt field bittern pan, chemical liquid storage, treatment tank, artificial lake and riverway etc.

Working Drawing

xiuhe xiuhe xiuhe xiuhe
xiuhe xiuhe xiuhe xiuhe

Specifications

Thicknesses mm 0.75 1 1.25 1.5 2 2.5 3
Densities g/cm³ ≥ 0.940
Roughness height ≥0.25
Tensile yield strength (longitudinal and transverse) N/mm ≥11 ≥15 ≥18 ≥22 ≥29 ≥37 ≥44
Tensile breaking strength (longitudinal and transverse) N/mm ≥8 ≥10 ≥13 ≥16 ≥21 ≥26 ≥32
Yield elongation (longitudinal and transverse) % ≥12
Elongation at break (longitudinal and transverse) % ≥100
Right angle tearing load (longitudinal and transverse) N ≥93 ≥125 ≥160 ≥190 ≥250 ≥315 ≥375
puncture strength N ≥ 200 ≥ 270 ≥335 ≥400 ≥ 535 ≥670 ≥800
Stress cracking under tensile load ≥300
Carbon black content % 2.0-3.0
Carbon Black Dispersibility No more than 1 out of 10 data at level 3, not allowed at levels 4 and 5
Atmospheric pressure oxidation induction time (OIT)min Atmospheric pressure oxidation induction time ≥ 100
High pressure oxidation induction time ≥ 400
85°C heat aging % ≥55
anti-ultraviolet ≥ 50

Pack and Ship

Packaging: Standard packaging or customer's requirements

Lead time: Within 10-15 days after receiving the deposit payment

Producing Capacity: Two 40ft Containers per week

xq xq xq xq