Papua New Guinea Texture and Smooth Coal Mining Pond Liner 1.0mm HDPE Geomembrane

Geomembranes use plastic movies as anti-seepage substrates, commonly which encompass polyvinyl chloride (PVC) and polyethylene (PE), EVA (ethylene/vinyl acetate copolymer). In tunnel applications, ECB (ethylene vinyl acetate modified asphalt combo geomembrane) is moreover designed and used.

Category:

Papua New GuineaTextured HDPE Geomembrane

Product Description

Introduction

Textured Geomembrane commonly refer to Geomembrane. with floor textures or uneven patterns, which are usually used for waterproofing, anti-seepage, or isolation purposes. This kind of Geomembrane can select fantastic textures in accordance to the required engineering necessities to amplify the adhesion and anti slip potential of the Geomembrane with different materials. When choosing textured Geomembrane., it is encouraged to reflect onconsideration on the particular engineering necessities and cloth houses comprehensively to make certain the overall performance and provider existence of the Geomembrane.

Video Showcase

 

Applications

  1. High strength: The textured geotextile has gone through exclusive therapy and has excessive tensile and tear strength, which can stand up to positive exterior masses and stresses.
  2. Good water resistant performance: The textured geotextile movie has first-rate water-resistant performance, which can successfully stop water infiltration and guard the engineering shape from water erosion.
  3. Corrosion resistance: Textured geotextiles are normally made of corrosion-resistant materials, which have the capability to face up to chemical corrosion and are appropriate for building below a range of harsh environmental conditions.

Working Drawing

xiuhe xiuhe xiuhe xiuhe
xiuhe xiuhe xiuhe xiuhe

 

Specifications

Thicknesses mm 0.75 1 1.25 1.5 2 2.5 3
Densities g/cm³ ≥ 0.940
Roughness height ≥0.25
Tensile yield strength (longitudinal and transverse) N/mm ≥11 ≥15 ≥18 ≥22 ≥29 ≥37 ≥44
Tensile breaking strength (longitudinal and transverse) N/mm ≥8 ≥10 ≥13 ≥16 ≥21 ≥26 ≥32
Yield elongation (longitudinal and transverse) % ≥12
Elongation at break (longitudinal and transverse) % ≥100
Right angle tearing load (longitudinal and transverse) N ≥93 ≥125 ≥160 ≥190 ≥250 ≥315 ≥375
puncture strength N ≥ 200 ≥ 270 ≥335 ≥400 ≥ 535 ≥670 ≥800
Stress cracking under tensile load ≥300
Carbon black content % 2.0-3.0
Carbon Black Dispersibility No more than 1 out of 10 data at level 3, not allowed at levels 4 and 5
Atmospheric pressure oxidation induction time (OIT)min Atmospheric pressure oxidation induction time ≥ 100
High pressure oxidation induction time ≥ 400
85°C heat aging % ≥55
anti-ultraviolet ≥ 50

Pack and Ship

Packaging: Standard packaging or customer's requirements

Lead time: Within 10-15 days after receiving the deposit payment

Producing Capacity: Two 40ft Containers per week

xq xq xq xq