Papua New Guinea Waterproof HDPE Geomembrane Liner Pond Liner Dam Liner

Geomembranes use plastic movies as anti-seepage substrates, commonly which encompass polyvinyl chloride (PVC) and polyethylene (PE), EVA (ethylene/vinyl acetate copolymer). In tunnel applications, ECB (ethylene vinyl acetate modified asphalt combo geomembrane) is moreover designed and used.

Category:

Papua New GuineaPond Liner

Product Description

Introduction

HDPE Geomembrane made from polyethylene polymer materials, through blowing or extruding technology, CE/ASTM/GB standards available. Our thickness ranges from 0.2-3mm; smooth, textured or bi-color surfaces available. HDPE Geomembrane main function is to prevent the liquid leakage and gas volatile. It is widely used in lining of pond reservoirs, canal, waste water, landfill, dams, Lakes, fish ponds and many other areas because HDPE Geomembrane is cost effectiveness and resistance against chemical and weather conditions.
By the way, except HDPE Geomembrane, we can also produce LDPE/EVA/PVC/EPDM materials geomembranes.

Video Showcase

 

Applications

1. Prevent leakage disposal in landfills, waste water, or in waste dregs disposing field.
2. Retain river bank, lake dam, mine, reservoir, tunnel. Working as liquid storage pools.
3. Prevent leakage in subway, basement, tunnel. Also, it prevents anti-salt leakage in roadbed, and other projects.
4. The plane and the vertical direction laying of dam and ground sill, LLDPE Geomembrane Liner is used in the construction fence and waste material fields.
5. Used in ground sill of road, highway, railway, and waterproof layer of swelling clay.
6. Prevent leakage on rooftop.

Working Drawing

xiuhe xiuhe xiuhe xiuhe
xiuhe xiuhe xiuhe xiuhe

 

Specifications

Thicknesses mm 0.75 1 1.25 1.5 2 2.5 3
Densities g/cm³ ≥ 0.940
Roughness height ≥0.25
Tensile yield strength (longitudinal and transverse) N/mm ≥11 ≥15 ≥18 ≥22 ≥29 ≥37 ≥44
Tensile breaking strength (longitudinal and transverse) N/mm ≥8 ≥10 ≥13 ≥16 ≥21 ≥26 ≥32
Yield elongation (longitudinal and transverse) % ≥12
Elongation at break (longitudinal and transverse) % ≥100
Right angle tearing load (longitudinal and transverse) N ≥93 ≥125 ≥160 ≥190 ≥250 ≥315 ≥375
puncture strength N ≥ 200 ≥ 270 ≥335 ≥400 ≥ 535 ≥670 ≥800
Stress cracking under tensile load ≥300
Carbon black content % 2.0-3.0
Carbon Black Dispersibility No more than 1 out of 10 data at level 3, not allowed at levels 4 and 5
Atmospheric pressure oxidation induction time (OIT)min Atmospheric pressure oxidation induction time ≥ 100
High pressure oxidation induction time ≥ 400
85°C heat aging % ≥55
anti-ultraviolet ≥ 50

Pack and Ship

Packaging: Standard packaging or customer's requirements

Lead time: Within 10-15 days after receiving the deposit payment

Producing Capacity: Two 40ft Containers per week

xq xq xq xq