Papua New Guinea Plastic Pond Liner Geomembrane 0.5mm 0.75mm 1mm 1.5mm HDPE Geomembrane Liner

Geomembranes use plastic movies as anti-seepage substrates, commonly which encompass polyvinyl chloride (PVC) and polyethylene (PE), EVA (ethylene/vinyl acetate copolymer). In tunnel applications, ECB (ethylene vinyl acetate modified asphalt combo geomembrane) is moreover designed and used.

Category:

Papua New GuineaPond Liner

Product Description

Introduction

High Density Polyethylene (HDPE) is the high density version of PE plastic and is harder and denser than the LDPE, but is less ductile, and lighter than water. Climax HDPE Film / Sheet / Liner / Geomembrane has proved to be a boon especially for developing countries like India by playing an important role to prevent the air and groundwater pollution. The best thing is that it can be easily moulded and welded together and the use of UV Stabilizers improves its weather resistance. High Density Polyethylene Geomembrane lives up to the expectations which are demanded in today's world of environmental engineering. Climax HDPE's prime motive is to keep the Nature clean. 

Video Showcase

 

Applications

1.landfill,sewage or control the waste residue seashores seepage.
2.Lake dam,tailings dams,sewage dam and reservoir,channel,storage of liquid pools(pit,ore)
3.The subway ,tunnel,anti-seepage lining of basement and tunnel.
4.To control the roadbed and other foundation saline seepage.

Working Drawing

xiuhe xiuhe xiuhe xiuhe
xiuhe xiuhe xiuhe xiuhe

 

Specifications

Thicknesses mm 0.75 1 1.25 1.5 2 2.5 3
Densities g/cm³ ≥ 0.940
Roughness height ≥0.25
Tensile yield strength (longitudinal and transverse) N/mm ≥11 ≥15 ≥18 ≥22 ≥29 ≥37 ≥44
Tensile breaking strength (longitudinal and transverse) N/mm ≥8 ≥10 ≥13 ≥16 ≥21 ≥26 ≥32
Yield elongation (longitudinal and transverse) % ≥12
Elongation at break (longitudinal and transverse) % ≥100
Right angle tearing load (longitudinal and transverse) N ≥93 ≥125 ≥160 ≥190 ≥250 ≥315 ≥375
puncture strength N ≥ 200 ≥ 270 ≥335 ≥400 ≥ 535 ≥670 ≥800
Stress cracking under tensile load ≥300
Carbon black content % 2.0-3.0
Carbon Black Dispersibility No more than 1 out of 10 data at level 3, not allowed at levels 4 and 5
Atmospheric pressure oxidation induction time (OIT)min Atmospheric pressure oxidation induction time ≥ 100
High pressure oxidation induction time ≥ 400
85°C heat aging % ≥55
anti-ultraviolet ≥ 50

Pack and Ship

Packaging: Standard packaging or customer's requirements

Lead time: Within 10-15 days after receiving the deposit payment

Producing Capacity: Two 40ft Containers per week