Papua New Guinea Naterproof Membrane Pond Liner 1.5mm 2.0mm 2.5mm 3.0mm

Geomembranes use plastic movies as anti-seepage substrates, commonly which encompass polyvinyl chloride (PVC) and polyethylene (PE), EVA (ethylene/vinyl acetate copolymer). In tunnel applications, ECB (ethylene vinyl acetate modified asphalt combo geomembrane) is moreover designed and used.

Category:

Papua New GuineaPond Liner

Product Description

Introduction

High Density Polyethylene (HDPE) is the excessive density model of PE plastic and is more difficult and denser than the LDPE, however is much less ductile, and lighter than water. Climax HDPE Film / Sheet / Liner / Geomembrane has proved to be a boon particularly for growing nations like India via taking part in an vital position to stop the air and groundwater pollution. The pleasant element is that it can be effortlessly moulded and welded collectively and the use of UV Stabilizers improves its climate resistance. High Density Polyethylene Geomembrane lives up to the expectations which are demanded in brand new world of environmental engineering. Climax HDPE's high purpose is to maintain the Nature clean. 

Video Showcase

 

Applications

1.landfill,sewage or manipulate the waste residue shorelines seepage.
2.Lake dam,tailings dams,sewage dam and reservoir,channel,storage of liquid pools(pit,ore)
3.The subway ,tunnel,anti-seepage lining of basement and tunnel.
4.To manipulate the roadbed and different basis saline seepage.

Working Drawing

xiuhe xiuhe xiuhe xiuhe
xiuhe xiuhe xiuhe xiuhe

 

Specifications

Thicknesses mm 0.75 1 1.25 1.5 2 2.5 3
Densities g/cm³ ≥ 0.940
Roughness height ≥0.25
Tensile yield strength (longitudinal and transverse) N/mm ≥11 ≥15 ≥18 ≥22 ≥29 ≥37 ≥44
Tensile breaking strength (longitudinal and transverse) N/mm ≥8 ≥10 ≥13 ≥16 ≥21 ≥26 ≥32
Yield elongation (longitudinal and transverse) % ≥12
Elongation at break (longitudinal and transverse) % ≥100
Right angle tearing load (longitudinal and transverse) N ≥93 ≥125 ≥160 ≥190 ≥250 ≥315 ≥375
puncture strength N ≥ 200 ≥ 270 ≥335 ≥400 ≥ 535 ≥670 ≥800
Stress cracking under tensile load ≥300
Carbon black content % 2.0-3.0
Carbon Black Dispersibility No more than 1 out of 10 data at level 3, not allowed at levels 4 and 5
Atmospheric pressure oxidation induction time (OIT)min Atmospheric pressure oxidation induction time ≥ 100
High pressure oxidation induction time ≥ 400
85°C heat aging % ≥55
anti-ultraviolet ≥ 50