PRODUCTS CENTER


Guyana Recyclable Raw Materials HDPE Liner with Better Price for Pond Liner

Geomembranes use plastic movies as anti-seepage substrates, commonly which encompass polyvinyl chloride (PVC) and polyethylene (PE), EVA (ethylene/vinyl acetate copolymer). In tunnel applications, ECB (ethylene vinyl acetate modified asphalt combo geomembrane) is moreover designed and used.

Category:

GuyanaPond Liner

Product Description

Introduction

HDPE Pond Liner is designed and made of excessive fantastic polyethylene resin with proportional carbon black antioxidant, anti-aging and UV-resistance substances which showcase impermeable and ultraviolet resistance properties. Compared with regular concrete and compacted clay, HDPE geomembranes are cost effective, environmental and effortless installation. they are extensively used for stable waste landfills,  waste containment, aquaculture and water remedy system, etc.

Video Showcase

 

Applications

1.Environmental Protection:

For example, landfills, sewage cure plants, strength plant regulating pools, industrial and medical institution strong wastes, etc.

2. Water Conservancy:

For example, seepage prevention, plugging, reinforcement, canal seepage prevention, vertical core wall, slope protection, etc.

3. Aquaculture Industry:

Intensive, industrialized aquaculture ponds, fish ponds, shrimp ponds lining, sea cucumber circle protection, etc.

4. Gardens:

Artificial lakes, rivers, reservoirs, golf pools, slope protection, greening lawns, waterproofing and moisture-proof.

5. Petrifaction:

Chemical plant, refinery, storage tank seepage control, chemical response tank, sedimentation tank lining, two liner, etc.

6. Agriculture:

Seepage manipulate of reservoirs, utility pools, reservoirs, irrigation systems, etc.

7. Salt Industry:

Salt pond, salt movie and salt pond plastic movie

Working Drawing

xiuhe xiuhe xiuhe xiuhe
xiuhe xiuhe xiuhe xiuhe

 

Specifications

Thicknesses mm 0.75 1 1.25 1.5 2 2.5 3
Densities g/cm³ ≥ 0.940
Roughness height ≥0.25
Tensile yield strength (longitudinal and transverse) N/mm ≥11 ≥15 ≥18 ≥22 ≥29 ≥37 ≥44
Tensile breaking strength (longitudinal and transverse) N/mm ≥8 ≥10 ≥13 ≥16 ≥21 ≥26 ≥32
Yield elongation (longitudinal and transverse) % ≥12
Elongation at break (longitudinal and transverse) % ≥100
Right angle tearing load (longitudinal and transverse) N ≥93 ≥125 ≥160 ≥190 ≥250 ≥315 ≥375
puncture strength N ≥ 200 ≥ 270 ≥335 ≥400 ≥ 535 ≥670 ≥800
Stress cracking under tensile load ≥300
Carbon black content % 2.0-3.0
Carbon Black Dispersibility No more than 1 out of 10 data at level 3, not allowed at levels 4 and 5
Atmospheric pressure oxidation induction time (OIT)min Atmospheric pressure oxidation induction time ≥ 100
High pressure oxidation induction time ≥ 400
85°C heat aging % ≥55
anti-ultraviolet ≥ 50

Pack and Ship

Packaging: Standard packaging or customer's requirements

Lead time: Within 10-15 days after receiving the deposit payment

Producing Capacity: Two 40ft Containers per week

xq xq xq xq